| Categories | Square Flat Washers |
|---|---|
| Model Number: | M16 |
| Place of Origin: | CHINA |
| MOQ: | 500KGS/Size |
| Payment Terms: | L/C, T/T, Western Union |
| Delivery Time: | 20days |
| Packaging Details: | plastic bag+carton+wood pallet |
| Material: | carbon steel , stainless steel |
| Size: | M6-M52 |
| Surface: | Zinc plated, HDG,Yellow |
| Port: | Shanghai, Ningbo, Zhapu |
| Garde: | 4.8,8.8,10.9,SS304,SS316 |
| Standard: | DIN,ISO,ANSI,GB,ASTM |
| Packing: | Bags,small box package,suit for shipping or according to requirement,small plain box,Bulk Carton |
| Type: | Flat Washer,Mechanical Parts,Flat Gasket,Hardware Fasteners |
High Quality DIN436-1990 Zinc Plated With Round Hole Square Flat
Washers M8,M10,M12
Product Description:
A washer is a thin plate with a hole typically in the middle that
is normally used to distribute the load of a threaded fastener,
such as a screw or nut. Other uses are as a spacer, spring wave
washer, preload indicating device, locking device, and to reduce
vibration. Washers usually have an outer diameter about twice
larger than their inner diameter. Washers are usually stainless
steel or carbon steel or plastic. High-quality joints require
hardened steel washers to prevent the loss of pre-load due to the
torque is applied
A washer is a thin plate (typically disk-shaped) with a hole
(typically in the middle) that is normally used to distribute the
load of a threaded fastener, such as a bolt or nut. Other uses are
as a spacer, spring (Belleville washer, wave washer), wear pad,
preload indicating device, locking device, and to reduce vibration
(rubber washer). Washers often have an outer diameter (OD) about
twice their inner diameter (ID), but this can vary quite widely.
Washers are usually metal or plastic. High-quality bolted joints
require hardened steel washers to prevent the loss of pre-load due
to Brinelling after the torque is applied.
Rubber or fiber gaskets used in taps (or faucets, or valves) to
stop the flow of water are sometimes referred to colloquially as
washers; but, while they may look similar, washers and gaskets are
usually designed for different functions and made differently.
Washers are also important for preventing galvanic corrosion,
particularly by insulating steel screws from aluminum surfaces.
Specification:
1. Material: Low Carbon steel, Mild Carbon steel, Stainless steel
2. Dimension: M3-M52, 3/16-24---2”
3. Grade: 4.8, 5.8, 6.8, 8.8, B7, 10.9
4. Coating: Plain, Black, Zinc Plated, HDG
5. Packing: Nylon bag, Carton ,pallet
6. Standard: DIN, ASTM/UNC,BSW,ISO,GB
7. Delivery: at least 20days
8. Port: Shanghai, Ningbo, Zhapu
9. Payment Terms: T/T, L/C
10. Name: High Quality DIN436-1990 Zinc Plated With Round Hole
Square Flat Washers M8,M10,M12
| Size | A | B | T | |||
| Max. | Min. | Max. | Min. | Max. | Min. | |
| 5 | 5.80 | 5.5 | 18 | 16.9 | 2.3 | 1.7 |
| 6 | 6.96 | 6.6 | 22 | 20.7 | 2.3 | 1.7 |
| 8 | 9.36 | 9 | 28 | 26.7 | 3.6 | 2.4 |
| 10 | 11.43 | 11 | 34 | 32.4 | 3.6 | 2.4 |
| 12 | 13.93 | 13.5 | 44 | 42.4 | 4.6 | 3.4 |
| 14 | 15.93 | 15.5 | 50 | 48.4 | 4.6 | 3.6 |
| 16 | 18.2 | 17.5 | 56 | 54.1 | 6 | 4 |
| 20 | 22.84 | 22 | 72 | 70.1 | 7 | 5 |
| 22 | 24.84 | 24 | 80 | 78.1 | 7 | 5 |
| 24 | 28.84 | 26 | 85 | 82.8 | 7 | 5 |
| 27 | 30.84 | 30 | 98 | 95.88 | 7 | 5 |
| 30 | 34 | 33 | 105 | 102.8 | 7 | 5 |
| 33 | 37 | 36 | 112 | 109.8 | 7 | 5 |
| 36 | 40 | 39 | 125 | 122.5 | 9.2 | 6.8 |
| 39 | 43 | 42 | 140 | 137.5 | 9.2 | 6.8 |
| 42 | 46 | 45 | 150 | 147.5 | 9.2 | 6.8 |
| 45 | 49 | 48 | 160 | 157.5 | 9.2 | 6.8 |
| 48 | 63.2 | 52 | 170 | 167.5 | 11.2 | 8.8 |
Application:
Flat washer, also known as plain washer, mainly iron plates punched
out, the general shape of a flat washer, a hole in the middle. The
pore size specifications according to customer requirements are
generally given. Flat washers generally thin pieces of various
shapes, to reduce friction, prevent leakage, isolate, prevent
loosening or dispersed pressure. Flat washers are mainly used to
reduce the pressure, when some parts of the tightening axial force
is large, easy to make dish washer pressed into, and then would be
able to increase the hardness of the material to resolve. Many
materials and structures have this part, for the performance of all
kinds of similar effect.
Bearing surface by a threaded fastener material and process
limitations, bolts and other fasteners little, so as to reduce the
stress bearing surfaces protect the connector surface, which
employs a gasket. Flat washers which spread a load and prevent
damage to the surface being fixed. Actually , a flat washer may be
used when the hole is a larger diameter than the fixing nut. A flat
washer with a large outer diameter. These are commonly used in
auto-body repair, sheet metal, plumbing, and electrical
applications. Washers are also important for preventing corrosion,
particularly by insulating steel screws from aluminum surfaces.
Advantages:
1. Good after sales service. Any small problem happening will be
solved at the most prompt time;
2. Many years of export experience;
3. Specifications list is available upon your request
4. Welcome to send enquiry, we will reply soon.
5. Prompt shipment with professional documents
6. Custom packing, with photo before shipment
7. High quality and competitive price.
|