| Categories | TDI Based Polyurethane |
|---|---|
| Brand Name: | EXCEEDCHEM |
| Model Number: | TDI-80/Polyether Polyurethane Prepolymer Shore A95-97 |
| Certification: | ISO9001:2008 |
| Place of Origin: | China |
| MOQ: | 1mt |
| Price: | FOB Qingdao usd3.0/kg |
| Payment Terms: | L/C, T/T |
| Supply Ability: | 3000mt/month |
| Delivery Time: | 5-8 work days |
| Packaging Details: | 20kg/drum; 200kg/drum |
| NCO%: | 6.50-6.70 |
| MOCA%: | 18.8-19.2 |
| Hardness: | Shore A95-97 |
| Base: | TDI-80/Polyether |
| Color: | colorless liquid |
| CAS NO: | 584-84-9 |
TDI 80 Polyurethane Prepolymer Used In The Preparation Of PU Bars
1. Description
This is a TDI-80 based polyether polyurethane prepolymer.
2. Characteristics
3. Applications
4. Typical properties
| Type | Appearance | Viscosity(mPa.s/85℃) | NCO% | Packing(kg/drum) |
| Liquid | 300-330 | 6.50-6.70 | 20/200 |
5. Operating Procedure
First, the prepolymer should be preheated in 80-85℃. Second, after vacumming, the prepolymer is to be mixed with melting MOCA evenly. Third, with degassing, casting into mould, and vulcanization,and then demould. Lastly, the finished product should be post vulcanized.
6. Reaction parameters
| Item | MOCA (%) | Gel time(min) | Mixing temperature(℃) | Post vulcanization(h) |
| Specification | 18.8-19.2 | 2.5-3 | 80/120 | 10 |
7. Finished products properties
| Item | Hardness(Shore A) | Tensile strength(MPa) | Tear strength(KN/m) | Rebounding(%) |
| Physical properties | 95-97 | 35-36 | 95-100 | 41 |
|